Fig. 8From: Platelet adhesion on commercially pure titanium plates in vitro III: effects of calcium phosphate-blasting on titanium plate biocompatibilityNumber of platelets adherent on CaP-blasted cp-Ti and plain SUS316L plates. After incubation for 60 min, the plates were rinsed and further incubated with CCK-8 for 90 min. The amount of converted formazan was quantified using a microplate reader at 450 nm. N = 4. P < 0.05 compared to SUS316Back to article page